Czochralski crystal growth furnace systems
CZ-CGF
CZ-CGF specification
D-120
D-100
D-120
- Crystal growth technique – The Czochralski method
- Furnace Сonstruction
- Type – 2-Zone
- Crucible – Dia. 120 mm, Height: 120 mm
- Heating height – 2×240 mm
- Atmosphere – Air
- Pressure – Atmospheric
- Temperature
- Maximal – 1.300 °C
- Continues – 1.150 °C
- Temperature control
- Accuracy – 0,1 °C
- Heating/Cooling rate – 0,04-100 °C/hour
- Crystal seed rod mechanism
- Pullin speed range – 0,03-10 mm/hour
- Max travel distance – 500 mm
- Rotation speed – 4-40 r/min
- Crystals Typical – BaB2O4, (BBO)LiNbO3, (LN)
- Power consumption
- Peak – 4 kW
- Continues – 1,9 kW
D-100
- Crystal growth technique – The Czochralski method
- Furnace Сonstruction
- Type – 2-Zone
- Crucible – Dia. 100 mm, Height: 150 mm
- Heating height – 2×150 mm
- Atmosphere – Air
- Pressure – Atmospheric
- Temperature
- Maximal – 1.100 °C
- Continues – 850 °C
- Temperature control
- Accuracy – 0,05 °C
- Heating/Cooling rate – 0,1-50 °C/hour
- Crystal seed rod mechanism
- Pullin speed range – 0,02-10 mm/hour
- Max travel distance – 400 mm
- Rotation speed – 1-50 r/min
- Crystals Typical – TeO2, LiB3O5 (LBO)
- Power consumption
- Peak – 3,5 kW
- Continues – 0,9 kW